Welcome to Guangdong Qinglong Construction Engineering Co., Ltd.!

Site Map   |  Contact Qinglong   | 

  • 中文
  • English
Qinglong UHPC & GRC

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

+86 760 8870 6348
+86 13902597531
Image display

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

资讯中心

ما آلية تسبب تآكل الفولاذ في تشقق مكونات GRC؟ آلية تمدد تآكل حديد التسليح في GRC والوقاية منها

2026-01-03 13:47:36

تصفح:

The mechanism by which steel bar corrosion causes GRC cracking is that rust expands in volume by 2-4 times, generating expansion stress of up to 30MPa. When the protective cover thickness is insufficient (<15mm) or compactness is inadequate, the corrosion-expansion stress exceeds the tensile strength of GRC (4-6MPa), resulting in cracks along the reinforcement, with crack width proportional to the corrosion rate.

Accelerated corrosion tests show that specimens with a 20mm protective cover developed 0.3mm cracks at a 5% corrosion rate, while specimens with a 15mm protective cover developed 0.5mm cracks at just a 3% corrosion rate. In one coastal project where sea sand was used (chloride ion content 0.08%), the steel bar corrosion rate reached 7% after 3 years of service, with cracks up to 1.2mm wide, making reinforcement work unavoidable.

Mechanical Analysis of Corrosion-Induced Expansion

Rust expands in volume by 2-4 times; expansion stress can reach 30MPa; these stresses cause cracking.

Quantification of Influencing Factors

Each 5mm reduction in protective cover advances the cracking time by 40%; chloride ion content above 0.06% accelerates corrosion 3-fold; these data guide design.

Key Protection Technologies

Protective cover thickness ≥20mm; adding corrosion inhibitors (dosage 2%-3%); these technologies effectively prevent rust.

Detection and Early Warning Methods

Half-cell potential testing; crack width monitoring; these methods enable timely detection.

Steel bar rust prevention is essential. Qinglong GRC's multiple protection ensures durability and safety.

0
ما آلية تسبب تآكل الفولاذ في تشقق مكونات GRC؟ آلية تمدد تآكل حديد التسليح في GRC والوقاية منها
اضغط لفترة طويلة على الصورة للحفظ / المشاركة
文章推荐
Image display

Homepage     |    Products     |    Project Cases     |    News Center     |    Joins     |    About Us     |    Contact Us

 Company Address: Room 302, No. 22 Dongming Road, Shiqi District, Zhongshan City, Guangdong Province

Business Hotline: +86 760 8870 6348      Mobile: +86 13902597531

Email address: qlfsgrc@163.com

 

 Scan to add WeChat

Copyright © Guangdong Qinglong Construction Engineering Co., Ltd. All Rights Reserved  . Recordation Number: 粤ICP备13069248号-24

التشاور عبر الإنترنت

مرحبًا ، الرجاء النقر فوق خدمة العملاء عبر الإنترنت للتواصل عبر الإنترنت!

بيانات المتصل
Contact number
+86 13902597531
امسح رمز الاستجابة السريعة ضوئيًا
رمز الاستجابة السريعة
Scan with WeChat
  • إلغاء
Add WeChat friend to learn more about the product
Use Enterprise WeChat
"Scan" to join the group chat
نسخ بنجاح!
Add WeChat friend to learn more about the product
I see.