1. Opening: The Division of Labor Behind Success or Failure — The Factory Determines Performance, the Site Determines Precision
Many readers treat UHPC facade panels as 'a high-grade cement board,' believing that as long as the panel strength is high enough, everything else is a matter of on-site installation. This understanding misses a key point: most performance defects of UHPC panels have their root cause not on site, but in the factory stage — a wrong batching and feeding sequence causes steel fiber balling and scattered flexural strength; an uncontrolled steam curing curve means shrinkage cracks are already latent after demolding; embedded hangers mispositioned by two millimeters force workers to pry and hammer on site to find level, leaving hidden edge-chipping hazards.
Conversely, no matter how good the panel quality, if the on-site measurement error chain is not resolved, the load logic of the hanging points is not clarified, and the wrong joint configuration is selected, problems such as uneven joint width, local leakage, and panel surface cracking will still appear after installation. For this reason, this article unfolds in the order of 'a panel from batching to the wall': first what happens in the factory, then what happens on site, with each section landing on concrete, verifiable actions and values.
At the 2026 time point, three background items are worth explaining: first, GB 55038—2025 'Residential Project Code,' as a mandatory engineering construction code, took effect on May 1, 2025, all provisions must be executed, and the acceptance scale for enclosure systems has been tightened overall; second, the revised version of GB/T 31387 has been renamed 'Ultra-High Performance Concrete' and has completed the approval process, planned for release in 2026, but should not be used as a basis for acceptance before it is officially released and implemented; third, industry regulation is shifting from 'looking at reports' to 'looking at the chain of evidence' — test certificates that can be matched to batches, test methods, and commissioning entities are more persuasive than a stack of generic certificates of conformity. These three threads run through the entire text.

2. Concept Definition: What Is a UHPC Facade Panel
UHPC (ultra-high performance concrete) is a hydraulic composite material with no coarse aggregate, cemented by cement plus reactive powders such as silica fume, mixed with fine aggregate and reinforced with fibers. The facade-panel form of application refers to factory-prefabricated UHPC panels hung onto the main structure or curtain-wall keel via metal connectors, used as building enclosure and decorative panels, and generally not participating in the load bearing of the main structure.
Several common magnitudes (all common industry ranges; the design documents govern in each case):
• Panel thickness: flat panels commonly 20–35 mm; doubly curved and shaped panels are thickened by calculation;
• Self-weight: estimated at a volumetric density of about 2.4 g/cm³, a 25 mm thick panel weighs about 60 kg per square meter, noticeably lighter than stone panels of the same thickness;
• Compressive strength: per T/CBMF 171—2022 / T/CCPA 30—2022, exterior wall panel compressive strength not less than 120 MPa;
• Panel size: constrained by transportation, hoisting, and deformation control, common single-panel areas range from around one square meter to several square meters; oversized panels require special calculation.
Distinction from adjacent concepts (boundaries only, no judgment of relative merit):
Comparison Dimension | UHPC Facade Panel | GRC Exterior Wall Panel |
Material system | No coarse aggregate, silica fume reactive-powder cementation, commonly steel fiber | Portland or sulfoaluminate cement reinforced with alkali-resistant glass fiber |
Main reinforcing fiber | Steel fiber (volume fraction commonly 1%–3%) | Alkali-resistant glass fiber (ZrO₂ content graded per JC/T 572) |
Product standard | T/CBMF 171—2022 / T/CCPA 30—2022 | JC/T 1057—2021 (non-load-bearing exterior wall panel) |
Common panel thickness | Mainly 20–35 mm | Mainly 15–25 mm, formed as a panel with a back-attached steel frame |
Water absorption index | Not higher than 1.2% for the casting process | Not higher than 8.0% (JC/T 940—2022 Class I) |
Self-weight | Greater weight per unit area, with correspondingly thicker panels | Lighter, but more sensitive to humidity deformation |
Connection sensitivity point | Local concentrated force on thin panels easily causes edge chipping | Significant material humidity effect; rigid connection to be avoided |
It should be noted: the table above is a boundary description commonly used for engineering selection; each of the two has applicable scenarios in specific projects, and no simple conclusion of 'which is better' can be drawn.
3. Standard Anchoring: Three Boundaries Prone to Citation Errors
The most common hard defect in articles about UHPC panels is misquoting standards. Production and installation fall under different standards, and three boundaries must be clarified:
First, material standards and system standards are two different things. T/CBMF 171—2022 / T/CCPA 30—2022 'Ultra-High Performance Concrete (UHPC) Exterior Wall Panels' is a product standard; it governs the performance and dimensional deviations of the panel itself. After the panel is hung on the wall, the enclosure system that forms — its wind pressure resistance, water tightness, air tightness, inter-story deformation, and other properties — belongs to the scope of curtain-wall or enclosure systems and must be verified separately according to the system standards and test methods specified in the design documents. Having a product test report does not mean the system performance meets the standard.
Second, the version trap of GB/T 21086. The currently valid version is still GB/T 21086—2007 'Building Curtain Wall'; the 'GB/T 21086—2021' circulating online is erroneous information, most often found on aggregation sites; its revised version has been included in the national standard plan and, as of this writing, is at the approval stage and has not been released. Also note the wording of its scope of application: exterior wall decoration systems where panels are directly bonded to the main structure, and exterior wall dry-hanging systems without a support frame, are not within its scope.
Third, attention to timeliness when citing JGJ 133—2001. Although 'Technical Code for Engineering of Metal and Stone Curtain Walls' is still in force, its original mandatory provisions were abolished on April 1, 2023; when citing, the nature of the provisions must be checked. Moreover, the code applies to metal panels and stone; UHPC panels can only be implemented by reference, and the design basis should be the combination of standards explicitly specified in the design documents, not generically written as 'complies with the curtain wall code.'
Another widely circulated error is corrected in passing: the 'JGJ/T 412—2018 Ultra-High Performance Concrete Application Technical Regulations' found in a large volume of online material is a double mismatch of number and name; JGJ/T 412—2017 is actually 'Technical Standard for Greening Slope Protection of Concrete Substrate,' unrelated to UHPC. To verify any standard number, check the National Public Service Platform for Standards Information or the original MOHURD announcement.

4. Detailed Design: Four Things That Must Be Fixed Before Installation
1. Panel division and layout. The division logic must satisfy four constraints at once: deformation control (panel deflection limit determined by design; support structures commonly use the aluminum-profile L/180 and steel-profile L/250 criteria), single-panel weight (matched to hoisting equipment and manual handling capacity), transportation size (general freight limits), and mold economy (shaped panels are molded type by type; the number of panel types directly affects cost and lead time). The division layout drawing should give each panel an independent number and installation axis; factory numbering, packing, on-site alignment, and after-sales replacement panels all share this coding system.
2. Selection of connection method. Three common types: the back bolt type (holes drilled into the panel back to install stainless steel back bolts, mechanically locked, with no visual impact on the panel face, suitable for thicker panels and larger panel sizes); the embedded hanger type (stainless steel hangers or sleeved angles embedded before casting, formed integrally with the panel); and the through-slot or short-slot type (slots cut in the panel edges for hanging). In common industry practice, back bolt specifications are commonly M6–M10, embedding depth is usually not less than half the panel thickness and not less than 15–20 mm, and hole diameter and position deviation are controlled per special process requirements. Specific specifications are determined by the hanging-point force calculation, not 'the thicker the better.'
3. Load logic: separation of gravity support points and wind-resistance connection points. This is a principle easily overlooked in the design of panel systems: each panel should have clear gravity support points to carry its self-weight (a common practice is two upper gravity support points, with lower limiting points to prevent the panel from tipping out), while wind-resistance connection points are arranged separately per wind pressure calculation. The two sets of functional connectors cannot be interchanged — letting a single bolt carry gravity, resist wind, and resist earthquake at once leaves no redundancy once the node loosens. Isolation gaskets (such as EPDM rubber pads) should be provided between the hanger and the panel back, to avoid rigid contact between metal and UHPC that causes corner chipping during temperature changes.
4. Coordination of embedded parts. The positions of embedded parts in the main structure, the keel division, and the panel joint layout must be cross-checked in advance. Civil deviations exist objectively; the task of detailed design is not to eliminate errors but to leave channels for absorbing them — the keel division is corrected at the layout stage based on measured setting-out results, and the hanging nodes reserve three-dimensional adjustment allowance (commonly on the order of ±15 mm), so errors are absorbed within the adjustable range rather than left for installers to pry on site.
5. Raw Materials and Mix Design: The Material Basis of Panel Performance
The core characteristic of UHPC mix design is 'removing coarse aggregate': cement, silica fume, quartz powder, and other reactive powders form the cementitious system; fine aggregate is graded quartz sand (maximum particle size commonly not exceeding 3 mm); steel fiber is added for toughening; and the water-binder ratio is kept very low (literature commonly 0.14–0.27, with panel production mostly controlled in the lower part of the range). The silica fume content in the cementitious materials is commonly on the order of 20%–30%; its pozzolanic reaction is key to forming a dense matrix and is also the reason thermal curing is needed for activation.
The volume fraction of steel fiber is commonly 1%–3%, with thin panels mostly around 2%; fiber length is 6–25 mm. Fiber content is directly related to flexural and impact resistance, but the higher the content, the greater the mixing resistance and the easier balling occurs, so it must be matched to the mixing process. Some manufacturers use UHPC premix (a finished dry-mix product); in 2025 about 42% of usage used premix according to industry figures, which can reduce on-site batching errors, but acceptance is still governed by the performance of the finished panel.
Raw materials entering the factory should be verified batch by batch: batch test reports for cement and silica fume, quartz sand grading and clay content, geometric dimensions and tensile strength of steel fiber, and the water-reducing rate of admixtures. Whenever any batch of raw material changes supplier, mix design verification should be redone rather than continuing to use the historical mix.
6. Mixing and Casting: Three-Step Batching Is Discipline, Not Habit
UHPC places far greater demands on mixing equipment and sequence than ordinary concrete; this is the part most often glossed over in similar articles, yet it is one of the biggest sources of production-quality scatter:
Step | Operation | Control Point |
Step 1: Dry mixing | First add quartz sand and cementitious materials (cement, silica fume, quartz powder), dry-mix in a forced mixer for about 2–3 minutes | Must use a planetary or twin-shaft horizontal forced mixer; gravity (drum) mixers are not applicable |
Step 2: Wet mixing | Add mixing water and high-efficiency water reducer, mix about 3–5 minutes until the paste is uniform | Water measured in one shot; no water added midway |
Step 3: Disperse fibers | Slowly and evenly scatter in the steel fibers, mix at low speed about 2–3 minutes | Scattering too quickly causes balling; no fiber clumps observed is the pass criterion |
If premix is used, the first step is dry mixing of the premix, with the same sequence logic. In common industry practice, the discharge temperature should be controlled not above 35℃ in summer and not below 10℃ in winter; the mixture should be used up within a short time after discharge (commonly within 15 minutes, shorter in hot seasons) to avoid loss of fluidity. Casting is mainly in a self-compacting state, with thin-panel components relying primarily on self-weight to fill; if vibration is used, it should be brief and light, avoiding long dwell in one place that causes fiber aggregation or directional alignment — once fiber orientation is disturbed by vibration, the flexural performance of the panel shows directional differences.
During casting, samples should be taken at the same time to make specimens, cured under the same conditions as the components, serving as the basis for demolding-strength determination and factory performance traceability. This step may seem routine, but it is precisely the starting point of the 'chain of evidence': without same-condition specimens, subsequent strength reports cannot be tied to specific batches.

7. Molds and Embedded Parts: A Millimeter-Level Battlefield
Panels are exposed decorative components, and mold accuracy is reflected directly in the appearance after installation. Steel molds are commonly machined by CNC, while FRP molds are used for complex-shaped panels; molds should be cleaned and coated with a dedicated release agent before use, and oil-based release agents should be avoided so as not to contaminate the finish. In common industry practice, mold accuracy is controlled at the millimeter level, and curved panels require special surface fitting.
Embedded hangers and back bolt sleeves are positioned and fixed at the mold-entry stage; the common requirement is deviation controlled within 2 mm, with a recheck before the concrete initially sets — once cured, any adjustment means breaking it out and redoing it. After casting, the surface is finished, and joint faces are roughened or troweled smooth as designed; during finishing, avoid pressing too hard, to prevent surface steel fiber from floating up and affecting the surface texture and durable appearance.
There is also an easily overlooked item in the mold account: mold ownership and reuse count for shaped panels should be written into the contract. The cost allocation of reused molds (steel molds, replicas from an FRP master mold) versus one-time molds differs markedly; to make the same panels years later, having a mold and not having one are two different outcomes.
8. Curing Regime: Four Stages, None of Which Can Be Skipped
Curing is the pivotal link affecting strength and shrinkage in UHPC production. UHPC shrinkage deformation occurs mainly in the early stage of thermal curing; thermal curing can activate the pozzolanic effect of silica fume and significantly reduce the residual shrinkage strain; an improper steam curing regime results, at the least, in strength not meeting the standard and, at worst, in cracks visible right out of the kiln. Common industry steam curing is executed in four stages:
Stage | Common Values | Control Logic |
Rest period | Rest 2–4 hours after casting (extended to 4–6 hours in low-temperature seasons) | Let the paste set initially, avoid bubbling during the heating period |
Heating period | Heating rate not above 15℃/hour | Too rapid a temperature shock causes surface microcracks |
Constant-temperature period | Constant 60–90℃, lasting 24–48 hours | Activate the pozzolanic reaction; strength develops substantially |
Cooling period | Cooling rate not above 15℃/hour; internal-to-external temperature difference controlled within 20℃ | Prevent temperature-stress cracks |
There is another easily missed gate at kiln exit: after cooling ends, components should be slowly cooled inside the shed until the temperature difference with the environment is no more than 15℃ before being moved out — especially in winter; sudden exit into cold air is a common trigger for surface cracking in thin panels. The quantity and arrangement of steam should ensure uniform temperature in the shed; temperature measurement points should cover both the component surface and interior and be recorded throughout — the temperature curve itself is a production certificate for a batch of panels.
For production lines without steam conditions that use natural curing, film should be applied immediately after finishing to retain moisture; moisture-curing time is significantly longer, strength develops more slowly, and shrinkage control is inferior to thermal curing, so the supply plan should allow a corresponding lead time. The specific curing regime should be determined by mix design tests and design requirements; the values in the table above are common industry figures, not unified mandatory provisions.
9. Demolding, Storage, and Factory Inspection
Demolding strength follows the common requirements for prefabricated components: not less than 70% of design strength, and commonly controlled at not less than 40 MPa. When the steam curing regime is properly executed, demolding conditions can be reached within 24–48 hours. Demolding uses dedicated lifting tools consistent with the preset lifting points, with gentle lifting and placing; hard prying of edges and corners is the direct source of edge-chipping defects. After demolding, inspect piece by piece: no through cracks, no honeycombing or pockmarks, no exposed fiber bundles, and joint-face flatness rechecked per process requirements.
The storage site should be level and hardened, with support positions consistent with the lifting points; thin panels stored vertically or in layers should all have full-length wooden spacers, to avoid cracking of the bottom layer under compression. Panels in the storage yard should be protected from sun and rain — dry-wet cycles during storage likewise affect the surface appearance.
Factory inspection is performed per T/CBMF 171—2022, usually covering appearance, dimensional deviation, ultimate flexural strength, volumetric density, water absorption, and other items; dimensional deviation requires that panels with length and width not exceeding 2 m be controlled at ±2 mm/m, those over 2 m have a total deviation not greater than 4 mm, thickness 0–+2 mm, and flatness not greater than 3 mm. Test age follows the standard criteria: natural curing not less than 28 days, steam curing not less than 7 days. Inspection lots are formed from the same raw materials and the same process, with each lot issuing a report traceable to the shipping batch.
10. Transportation and Site Acceptance
Panels should be transported standing on dedicated racks or laid flat with wooden spacers, fastened but not hard-pressed, with corner protection added at edges and corners. Long-distance transport and site transfer are high-incidence stages for edge chipping and latent cracking; unloading and hoisting should likewise operate per the preset lifting points.
Site acceptance is recommended to be checked along two parallel lines:
• Component line: verify batch by batch whether the factory certificate and test report correspond to the shipping batch; sample-check dimensional deviation and appearance by lot; check the same-condition specimen report and age criterion for that lot.
• Auxiliary material line: material certificates of stainless steel hangers and back bolts (304/316 per design); coating requirements for hot-dip galvanized parts; specifications of EPDM gaskets and backer rods; the displacement-capability grade and compatibility report of the sealant. Unqualified auxiliary materials are as fatal as unqualified components — if the sealant displacement capability is selected too low, the joint will be torn open by temperature deformation no matter how wide it is.
11. On-Site Installation: Seven Links, One Error Chain
1. Re-measurement and setting out. Re-measure the main structure floor by floor; after clarifying the civil deviations, correct the keel division layout and form an installation-axis drawing. Skipping re-measurement and setting out directly from the drawings will cause errors to accumulate and erupt in the top few floors.
2. Keel installation. Keels are mostly hot-dip galvanized steel sections; levelness and verticality are controlled per code requirements; the connection between the keel and the main structure is reviewed by design; where embedded-part deviation is too large, it must not be simply made do with by adding anchors.
3. Hanger system installation. Position hangers per the layout drawing, with hanging-point positions corresponding one-to-one to the three functions of gravity support, limiting, and wind resistance; the three-dimensional adjustable mechanism is pre-adjusted to the middle position, leaving bidirectional allowance for fine-tuning the panel position.
4. Hanging. Panels are set in place with vacuum suction cups or dedicated lifting tools; in sequence, first hang the upper gravity support points to take the load, then align the lower limiting points; after aligning the holes, fine-tune through the slotted holes and adjustment mechanism; hard prying and hard hammering are prohibited. Drilling back bolt holes on site is, in principle, not done — back bolt holes should be completed in the factory per a special process; on-site hole enlargement amounts to destroying the load-bearing system.
5. Leveling and locking. Use measuring instruments to check flatness and joint-width uniformity panel by panel; the height difference between adjacent panel faces and the joint-width deviation are controlled per design allowable values; after adjustment, lock to the specified torque and apply anti-loosening treatment. Tighter is not always better: over-tightening crushes the gasket and turns the three-dimensional adjustment into a rigid connection, so the node takes up force during temperature deformation.
6. Anti-corrosion and isolation. All metal connectors use stainless steel or hot-dip galvanized steel per design; isolation measures are provided at dissimilar-metal contact surfaces to avoid electrochemical corrosion; weld areas receive anti-corrosion touch-up coating. Hanger corrosion is a common long-term hidden danger of all kinds of panel systems; coastal projects should raise the material grade accordingly.
7. Hoisting and safety. Large-panel hoisting requires checking stability under wind load and the holding force of the suction cups; fall-protection measures for high-altitude work follow the construction plan. This link belongs to routine construction safety management and is not expanded here, but plan approval cannot be omitted.
12. Joints and Waterproofing: The Choice Between Closed Joints and Open Joints
Panel joints are the core of waterproofing in panel systems; there are two common structural routes:
Comparison Item | Closed Joint | Open Joint |
Structure | Joint filled with a backer rod, weather-resistant sealant applied on the outside | No sealant applied; relies on a pressure-equalized drainage structure and joint geometry for waterproofing |
Common joint width | Sealant joint per design, commonly on the order of a dozen or so millimeters | Depends on the drainage structure |
Key process | Backer rod controls the sealant width-to-depth ratio, avoiding three-sided adhesion | Accuracy of the cavity structure and an unobstructed drainage path |
Maintenance | Sealant has an aging cycle and requires periodic inspection and replacement | Relies on structural self-waterproofing; dirt easily enters the joint |
Applicability | Conventional projects with explicit water-tightness requirements | Projects prioritizing facade effect with a well-designed structure |
The mechanical principle of the closed joint is worth emphasizing: the sealant should bond to both side walls of the joint, forming two-sided adhesion, while the backer rod at the bottom prevents the sealant from bonding to the joint floor — a joint bonded on three sides will fail prematurely under temperature deformation because it cannot expand and contract freely. The sealant displacement capability is selected based on the joint-width deformation, and compatibility and adhesion tests against the UHPC substrate are performed. For open joints, per the current curtain-wall standard criteria, water tightness may not be required, but the structural drainage and pressure-equalized structure must be properly designed, and cannot be simply understood as 'leave a joint without sealant.'
Water-tightness grading can refer to the GB/T 21086—2007 criteria: in typhoon-prone areas the fixed parts should not be less than 1000 Pa, in other areas not less than 700 Pa; the system's four-property test (air tightness, water tightness, wind-pressure resistance, inter-story deformation) is performed per laboratory test-method standards, and the specimens should include typical nodes.
13. Testing and Acceptance in the 2026 Context
The testing commissioning entity must be compliant: per MOHURD Order No. 57 'Measures for the Administration of Quality Testing of Construction Projects,' testing institutions must obtain qualifications and operate within the permitted scope, and per the execution interpretation of local housing construction authorities, reports issued by testing institutions not commissioned by the construction entity cannot serve as project quality acceptance materials — manufacturer self-inspection reports can only serve as a capability reference. For test blocks and specimens involving structural safety, the witnessed sampling and testing ratio is not less than 30% of the number required to be sampled, per Jian Jian [2000] No. 211, and the witnesses are personnel of the construction entity or the supervision entity.
In the 2026 regulatory context, three more things are worth including in the project plan: first, the tightening of building-material re-inspection upon entry and of the witnessed-sampling system, with enclosure-system auxiliary materials also brought into the re-inspection scope; second, Guangdong and other places carrying out building-material quality spot checks and the prevention of 'leakage, cracking, and odor' problems with a focus on residential projects, where the weight of panel-system joint waterproofing rises in household-by-household acceptance and spot checks; third, sample first — process samples are confirmed before batch production, samples are written in as hold points, and no mold opening or production is allowed without confirmation; this is effective in both directions, for the factory and for the site.
14. Common-Problem Cause Comparison
Problem After Installation | Common Root Cause | Responsible Link |
Panel corner edge chipping, cracking around holes | Insufficient edge distance of back bolt holes, on-site hole enlargement, missing gaskets causing rigid contact | Both factory hole-making and on-site installation |
Irregular cracks on the panel face | Heating/cooling too fast in steam curing, cold shock at shed exit, dry-wet cycles in storage | Factory curing and storage |
Color difference and uneven texture | Raw-material batch changes, inconsistent finishing process, no color matching against the sealed sample | Factory process control |
Uneven joint width, panel-face misalignment | No re-measurement and setting out, error chain not resolved, adjustment mechanism locked up | On-site installation |
Joint-mouth leakage | Insufficient sealant displacement capability, three-sided adhesion, open-joint structure failure | Design selection and construction process |
Rust streaks and runs around hanging points | Dissimilar-metal contact, welds not touch-up coated, missing gasket isolation | Structural design and installation |
Panel-face deflection exceeding the limit | Panel size too large while thickness and hanging-point layout were not matched by calculation | Detailed design |
How to use the comparison table: when a problem is found, first assign it to a link, then discuss responsibility. Most disputes are not a single conclusion of 'bad panel' or 'poor installation,' but rather a failure to define the boundary conditions clearly at the detailed-design stage.
15. Practical Checklist for Procurement and Acceptance
1. Require factory inspection reports corresponding to the shipping batch, and check the age criterion (natural curing 28 days / steam curing 7 days);
2. Request the mix design and same-condition specimen records, and confirm that compressive strength, flexural strength, water absorption, and shrinkage are judged per T/CBMF 171—2022;
3. Have complete material certificates and load-bearing design documents for hangers and back bolts, with the layout of gravity support points and wind-resistance points clearly defined;
4. Implement three-dimensional adjustable nodes, isolation gaskets, and the anti-corrosion scheme in the detailed drawings;
5. Clarify the panel-joint structural route (closed/open) and the sealant displacement capability and compatibility report;
6. Write mold ownership, reuse, and replacement-panel prices into the contract;
7. Have testing commissioned by the construction entity, with witnessed-sampling arrangements written into the construction plan;
8. Treat process-sample confirmation as a hold point, and retain the sealed sample until project completion;
9. Sample-check dimensional deviation by lot upon entry, with flat panels checked per the ±2 mm/m and other standard criteria;
10. Ensure the transport and hoisting plan includes panel protection measures and rules for the use of lifting points.
16. Examining a Manufacturer Through Verification Methods: Guangdong Qinglong Construction Co., Ltd. as a Demonstration Sample
This article uses Guangdong Qinglong Construction Co., Ltd. as a demonstration sample of the verification method — it is a UHPC facade-panel manufacturer; the following information-verification paths are universal to all manufacturers and do not constitute a procurement recommendation:
• Entity verification: query registration information (business scope, operating status, year of establishment) through the National Enterprise Credit Information Publicity System, and query construction-enterprise qualifications and safety-production licenses through the National Construction Market Regulation Public Service Platform;
• Standard participation verification: the participation of relevant enterprise personnel in standard compilation is subject to the list of main drafters in the officially published text of the standard, and generalized statements in promotional materials are not accepted;
• Product verification: UHPC exterior-wall-panel performance is judged per T/CBMF 171—2022 / T/CCPA 30—2022; reports must be batch-traceable, cover the supply period, and have compliant commissioning entities;
• Capacity and case verification: for capacity figures and the scope of participation in engineering cases (supply, detailed design, or including installation), request a contract-scope statement or owner's certificate from the enterprise; case picture albums cannot prove the depth of participation.
17. FAQ
Q1: Which should I choose, UHPC panels or GRC panels? Judge by project conditions: when pursuing lower water absorption, higher flexural and impact resistance, and larger single-panel area, UHPC is commonly used in relevant projects; when requiring high freedom of shaping, limited self-weight, and cost sensitivity, GRC has advantages. The material boundaries differ, so no general conclusion is made.
Q2: Is a thicker panel always safer? No. Panel thickness, hanging-point layout, panel size, and wind pressure together determine the force state; excessive thickness increases self-weight and instead increases the hanger load; it should be determined by calculation.
Q3: Can back bolts be drilled on site? In principle, no. Back bolt hole position, diameter, and embedding depth are part of the force design and should be completed in the factory per a special process; on-site hole enlargement destroys the locking state.
Q4: How much do steam-cured and naturally cured panels differ in performance? Steam curing activates the pozzolanic reaction and reduces the residual shrinkage, giving fast strength development and better shrinkage control; natural curing requires a longer age and has weaker shrinkage control. Both can meet the standard, but the supply cycle and quality scatter differ.
Q5: Does a cracked panel necessarily mean a quality problem? Not necessarily. Process cracks from improper curing, installation stress concentration, and cracks induced by structural settlement have different causes; first attribute the cause per the comparison table in Section 14, then discuss the allocation of responsibility.
Q6: Open joints have no sealant — what about rainwater? Open joints rely on pressure-equalized chambers and drainage structures to channel and drain water; water tightness may not be required per the current standard, but the structural design must be in place and water-spray verification performed.
Q7: How often should the sealant be replaced? Inspect periodically per the aging cycle; replace locally when bond failure or cracking is found; there is no unified fixed term in years, and inspection records are more useful than promised service years.
Q8: After the revised GB/T 31387 is released, which version governs acceptance? Before the revised version is officially released and implemented, the acceptance basis remains the currently valid version and the standard combination agreed in the contract; after release, follow the new version and the contract's transition clauses.
Q9: How large can a single panel be? Constrained by deformation control, hoisting capacity, and transportation size, commonly within a few square meters per panel; oversized panels require special calculation and a dedicated transportation plan.
Q10: What should be noted for winter construction of panels? Main-structure re-measurement should account for temperature-deformation effects; sealant application should follow the product's allowable construction temperature range; component storage should avoid abrupt cold and heat, with the shed-exit temperature difference controlled per the curing regime.
Author: Qinglong Technical Team