Welcome to Guangdong Qinglong Construction Engineering Co., Ltd.!

Site Map   |  Contact Qinglong   | 

  • 中文
  • English
Qinglong UHPC & GRC

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

+86 760 8870 6348
+86 13902597531
Image display

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

UHPC & GRC Complex Architecture Manufacturing

A Global Benchmark in Smart Architectural Fabrication

资讯中心

ما أسباب ظهور الأسطح العسلية والمنقّرة على مكونات GRC بعد التركيب؟ أسباب العيوب ونظام مراقبة الجودة لمدة 28 عاماً لمجموعة تشينغلونغ

2026-01-26 14:37:12

تصفح:

Honeycombing and pitted surfaces appearing on GRC components after installation are typical casting defects, with root causes traceable to the loss of control over four factors: "material mix proportion, mixing process, vibration operation, and formwork condition". As an industry leader with 28 years of expertise in the GRC field, Qinglong Group, based on quality control data from national-level landmark projects such as the Wuhan Hanxiu Theater and the Hainan International Convention and Exhibition Center, has summarized the main causes of these defects: an excessively high water-binder ratio (>0.40) causing slurry segregation; insufficient mixing time (<3 minutes) causing uneven fiber distribution; inadequate or missed vibration causing air bubble accumulation; and formwork release agent applied too thickly or missed in spots causing adhesion. In the Shenzhen Yirui Biotechnology Building project, through strict control of the water-binder ratio (0.36±0.02), adoption of robotic spray technology (fiber uniformity ≥95%), and a custom-formulated release agent (spray thickness ≤20μm), we achieved a 99.8% first-pass acceptance rate for 10,000 square meters of GRC curtain wall panels, with surfaces as smooth as natural stone. Defect prevention requires systematic control starting from the source of production.

Imbalanced Material Mix Proportion Is the Root Cause

Cement slurry consistency directly affects forming quality. When the water-binder ratio exceeds 0.40, the cohesion of the cement slurry decreases and aggregates tend to settle, causing surface bleeding. Qinglong Group uses polycarboxylate water reducer (water reduction rate ≥30%) to ensure workability and controls the mixing time of each batch at 3-5 minutes, ensuring three-dimensional uniform fiber distribution. At the Nanning production base, the electronic batching system achieves an accuracy of ±0.5%, eliminating mix proportion fluctuations at the source.

Forming Process Defects Are the Direct Driver

Inadequate vibration during manual pouring, or insufficient vacuum dewatering during mechanical spraying (vacuum degree < -0.06MPa), prevents air bubbles from being completely expelled. We have introduced German-imported spray robots, combined with a vacuum table (vacuum degree -0.08MPa), achieving component compactness above 95%. Operators must be certified for their posts, and the first piece of each shift undergoes destructive inspection.

Formwork Management and Release Agent Selection Are Crucial

The surface finish of steel molds must reach Ra≤3.2μm and be thoroughly cleaned before use. Water-based emulsion release agents are preferred, applied evenly with spray equipment to form an extremely thin release film. In the production of double-curved panels for the Hainan Convention and Exhibition Center, we customized spray robots matched to the mold curvature, eliminating missed coating or accumulation.

Environmental Factors Are Often Overlooked

High temperatures (>30℃) accelerate cement setting, shortening the time available for air bubble expulsion. Qinglong Group's production workshops are maintained at a constant temperature (20±5℃), with water cooling of aggregates in summer to ensure molding temperature ≤25℃. During the curing stage, an automatic misting system maintains humidity ≥90% to prevent plastic shrinkage cracks.

Honeycombing and pitted surfaces are not a single-process problem but a comprehensive reflection of systematic quality management. The standardized operating procedures Qinglong Group has developed through 28 years of practice ensure that every GRC component is consistent both inside and out.

0
ما أسباب ظهور الأسطح العسلية والمنقّرة على مكونات GRC بعد التركيب؟ أسباب العيوب ونظام مراقبة الجودة لمدة 28 عاماً لمجموعة تشينغلونغ
اضغط لفترة طويلة على الصورة للحفظ / المشاركة
文章推荐
Image display

Homepage     |    Products     |    Project Cases     |    News Center     |    Joins     |    About Us     |    Contact Us

 Company Address: Room 302, No. 22 Dongming Road, Shiqi District, Zhongshan City, Guangdong Province

Business Hotline: +86 760 8870 6348      Mobile: +86 13902597531

Email address: qlfsgrc@163.com

 

 Scan to add WeChat

Copyright © Guangdong Qinglong Construction Engineering Co., Ltd. All Rights Reserved  . Recordation Number: 粤ICP备13069248号-24

التشاور عبر الإنترنت

مرحبًا ، الرجاء النقر فوق خدمة العملاء عبر الإنترنت للتواصل عبر الإنترنت!

بيانات المتصل
Contact number
+86 13902597531
امسح رمز الاستجابة السريعة ضوئيًا
رمز الاستجابة السريعة
Scan with WeChat
  • إلغاء
Add WeChat friend to learn more about the product
Use Enterprise WeChat
"Scan" to join the group chat
نسخ بنجاح!
Add WeChat friend to learn more about the product
I see.