The durability of UHPC products is mainly reflected in indicators such as impermeability, frost resistance, carbonation resistance, and corrosion resistance. Premium products have a chloride ion diffusion coefficient ≤2.0×10⁻¹²m²/s, frost resistance grade ≥F300, and 50-year carbonation depth ≤5mm. Through low-alkali cement, optimized admixtures, and innovative curing processes, Qinglong UHPC achieves durability indicators 30%-50% better than national standards, with a service life exceeding 100 years.
Comparative experiments show: under the same harsh environment (Cl- concentration 3.5%, 300 freeze-thaw cycles), Qinglong UHPC has a mass loss rate ≤0.5% and relative dynamic elastic modulus ≥85%; ordinary products have a mass loss rate ≥1.5% and dynamic elastic modulus ≤70%. Ten years of tracking data from a coastal project confirm the outstanding durability of Qinglong UHPC.
Premium products have an impermeability grade ≥P12 with penetration height ≤10mm; ordinary products are P8-P10 with penetration height 15-25mm. Impermeability determines the durability of structures in corrosive environments.
Premium products show mass loss ≤5% after 300 freeze-thaw cycles; ordinary products show surface spalling after just 150 cycles. Frost resistance is a key indicator for applications in cold regions.
Premium products have an annual carbonation depth growth ≤0.1mm and ≤5mm over 50 years; ordinary products grow 0.2-0.3mm per year. Carbonation performance affects the protection of steel reinforcement.
Premium products show no rust after 360 days in 5% NaCl solution; ordinary products develop rust spots after 180 days. Corrosion resistance ensures service life in harsh environments.